    Has anyone seen anything like this happen to their prints? I've checked the extruder for a jam but it seems to be fine. I'm printing at 215C with PLA.

    Notice there's also a small amount of bowing on the sides. Could that be a heated bed issue? I print with the bed at 40C.
     

    Attached Files:

  2. Kadows

    Kadows Member

    Joined:
    Mar 4, 2014
    Messages:
    34
    Likes Received:
    10
    What % infill are you using? Or maybe its under extrusion?
     
  3. mark tomlinson

    mark tomlinson ༼ つ ◕_ ◕ ༽つ
    Staff Member

    Joined:
    Feb 21, 2013
    Messages:
    23,917
    Likes Received:
    7,338
    How many top layers are you using?
    The default is ... 2 or 3 (at 0.2mm)
    You might want more than that :)
     
  4. Mike Kelly

    Mike Kelly Volunteer

    Joined:
    Mar 11, 2013
    Messages:
    6,967
    Likes Received:
    2,277
    I generally suggest 1-1.5mm top layer height. IE for .2mm that'd be 5 top layers, or for .1mm that'd be 10-15
     